摘要:<p style="margin:0pt;text-align:left;"> <span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">西安不锈钢焊接点氧化层怎么去除</span></span> </p> <p style="margin:0pt;text-align:left;"> <span style="font-family:Calibri;font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;mso-fareast-font-family:宋體(tǐ);"><span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">西安不锈钢焊接主要是用(yòng)在接口处,两根不锈钢管如要进行对接,就会用(yòng)上電(diàn)焊方法,我们在选用(yòng)焊材的时候,一定要选择与不锈钢材质匹配的焊材,小(xiǎo)编不建议采用(yòng)碳钢焊材焊接不锈钢。電(diàn)焊不锈钢制品件的验收主要是检查焊接处的黑色氧化铁的存在以及除去方法。</span></span></span> </p> <p style="margin:0pt;text-align:left;"> <span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">電(diàn)焊焊接时温度较高,焊接处焊条熔化后当即与不锈钢制品焊接熔化在一起的同时,其表面也同时被氧化成黑色的三氧化二铁和四氧化三铁的焊渣,这层氧化铁在酸中极难溶解,若在酸中过長(cháng)时间浸蚀,则未焊接部位又(yòu)会糟到过腐蚀,既影响到镀层的正常沉积,又(yòu)会使不锈钢制品镀件的理(lǐ)化性能(néng)遭到影响。</span>)</span> </p> <p style="margin:0pt;text-align:left;"> <span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">方法一:我们可(kě)以先采用(yòng)*实用(yòng)的方法,那就是用(yòng)洗衣粉加水稀释之后,侵泡焊接处,再用(yòng)清水冲洗。如果焊接点氧化层不能(néng)去掉,我们可(kě)以采用(yòng)硫酸稀释之后侵泡,因為(wèi)硫酸具有(yǒu)强腐蚀性,所以我们一定要控制好侵泡时间,一般不能(néng)过長(cháng),然后再用(yòng)清水冲洗即可(kě)。</span></span> </p> <p style="margin:0pt;text-align:left;"> <span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">方法二:制作一把带尖头的头敲,头敲光滑平整,没有(yǒu)凹陷或者尖锐的地方,把所到之处氧化皮脱落。</span></span> </p> <p style="margin:0pt;text-align:left;"> <span style="font-family:宋體(tǐ);font-size:10.5pt;mso-spacerun:&quot;yes&quot;;mso-ascii-font-family:Calibri;mso-hansi-font-family:Calibri;mso-bidi-font-family:&quot;Times New Roman&quot;;mso-font-kerning:1.0000pt;"><span style="font-family:宋體(tǐ);">方法三:采用(yòng)去镀的方法来去除焊接点氧化层,研究了氧化层的组成,我们可(kě)以先将氧化层的表皮进行预处理(lǐ),采用(yòng)碱性硝酸盐熔融使得氧化层变得松软,然后在清洗焊接点,达到焊接点平滑,清洁的目的。</span></span> </p>

西安不锈钢焊接点氧化层怎么去除

西安不锈钢焊接主要是用(yòng)在接口处,两根不锈钢管如要进行对接,就会用(yòng)上電(diàn)焊方法,我们在选用(yòng)焊材的时候,一定要选择与不锈钢材质匹配的焊材,小(xiǎo)编不建议采用(yòng)碳钢焊材焊接不锈钢。電(diàn)焊不锈钢制品件的验收主要是检查焊接处的黑色氧化铁的存在以及除去方法。

電(diàn)焊焊接时温度较高,焊接处焊条熔化后当即与不锈钢制品焊接熔化在一起的同时,其表面也同时被氧化成黑色的三氧化二铁和四氧化三铁的焊渣,这层氧化铁在酸中极难溶解,若在酸中过長(cháng)时间浸蚀,则未焊接部位又(yòu)会糟到过腐蚀,既影响到镀层的正常沉积,又(yòu)会使不锈钢制品镀件的理(lǐ)化性能(néng)遭到影响。)

方法一:我们可(kě)以先采用(yòng)*实用(yòng)的方法,那就是用(yòng)洗衣粉加水稀释之后,侵泡焊接处,再用(yòng)清水冲洗。如果焊接点氧化层不能(néng)去掉,我们可(kě)以采用(yòng)硫酸稀释之后侵泡,因為(wèi)硫酸具有(yǒu)强腐蚀性,所以我们一定要控制好侵泡时间,一般不能(néng)过長(cháng),然后再用(yòng)清水冲洗即可(kě)。

方法二:制作一把带尖头的头敲,头敲光滑平整,没有(yǒu)凹陷或者尖锐的地方,把所到之处氧化皮脱落。

方法三:采用(yòng)去镀的方法来去除焊接点氧化层,研究了氧化层的组成,我们可(kě)以先将氧化层的表皮进行预处理(lǐ),采用(yòng)碱性硝酸盐熔融使得氧化层变得松软,然后在清洗焊接点,达到焊接点平滑,清洁的目的。